Abstract

Abstract Magnetic properties and microstructure were investigated in Sm 17.24 Co 66.20 Cu 8.28 Fe 8.28 ribbons melt-spun at different wheel speeds of 5, 15, 30, 40 and 50 m/s. X-ray diffraction studies revealed that the ribbons melt-spun at lower wheel speed ( 7 , Sm 2 Co 7 and SmCo 5 , while higher wheel speed ribbons exhibited single phase SmCo 5 . The coercivity was found to increase with increase of the wheel speed. A high coercivity of ∼33 kOe was obtained in ribbon prepared at 50 m/s.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.