Abstract

In order to study the change of each phase and the influence of single oxide during the consolidation of pellets. A systematic thermodynamic calculation was carried out through the phase diagram to study the influence of five oxides (CaO, SiO2, Fe2O3, Al2O3 and MgO) on the phase equilibrium of the hematite pellet system. The results show that the content of CaO has the most significant effect on the content of liquid phase and SPINA. There are critical values for the influence of SiO2 and CaO on the Ca3Fe2Si3O12 phase, which are 3.5% and 3.0%, respectively. Through in-situ heating experiments, XRD-Rietveld and SEM-EDS, the macro morphology and phase composition of the hardened samples were compared and analyzed. Finally, a multiple regression model is used to predict the liquid content of hematite pellets, which is effective in predicting the phase component.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.