Abstract
The bioactive coatings were prepared by laser cladding CaO–ZrO2–SiO2 system coatings on titanium alloy (Ti6Al4V). The cross-section morphologies of the coating are cellular crystal and cellular-dendrite structure. With the increase of ZrO2 content, the structure becomes coarse. The coating is mainly composed of CaTiO3, CaO, α-Ca2(SiO4), SiO2 and TiO2. When 5mol% ZrO2 was added, CaZrO3 appears. With the increase of ZrO2 content, ZrO2 appears and CaO disappears. The surface of these coatings are coarse, accidented and partial porous. After soaking in simulated body fluid (SBF), apatite is formed on the coating surface.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.