Abstract

Two series of siloxane-urethane copolymers were prepared from polydimethylsiloxane (PDMS) with a molecular weight of 1000 or 1800 which was used as a soft segment, 4,4′-diphenylmethane diisocyanate (MDI) and 1,4-butanediol (1,4-BD). Differential scanning calorimetry (DSC) demonstrated that the position (Tgs) and breadth (ΔB) of soft-segment glass transition of copolymers remained constant as the hard-segment content increased. Heat capacities at soft-segment glass transition of the copolymer (ΔCp) were 0.195∼0.411 J/g○C and heat capacities of pure PDMS (ΔCp0) were 0.571∼0.647 J/g○C, leading to the various ΔCp/ΔCp0 ratios. The ΔCp/ΔCp0 ratios decreased as the increasing of hard-segment content, showing poor phase separation. The FTIR spectrum confirmed the occurrence of hydrogen bonding in ether end-group of pure PDMS. The ether group of the soft segment led to interfacial mixing between soft and hard segments. The tan δ of the soft segment determined by dynamic mechanical testing (DMA) also identified the mixing of soft and hard segments. The mechanical properties of the copolymer were directly related to either the soft and hard segment contents or the chain lengths of soft and hard segments. The hard segment that reinforced the soft segment and interfacial thickness between soft and hard segment dominated the mechanical properties.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.