Abstract

We investigate the magnetic properties of CoSiB (1 5-Å-thickness)/Pd (Pd thickness = 8, 11, 14, 17, 20, 24, 27, 29 and 33 Å)/CoSiB (15-Å-thickness) trilayer thin films. The CoSiB-layer thickness was fixed to 15 Å, while the Pd-layer thickness was varied from 8-33 Å. In this paper, we present a new type of thin film containing amorphous Co75Si15B10 and Pd. We investigate the magnetic properties of a fabricated CoSiB/Pd/CoSiB trilayer thin film with perpendicular magnetic anisotropy, and determine the correlation between the magnetic properties and the nonmagnetic Pd-layer thickness. With increasing Pd-layer thickness, both the coercivity and the saturation magnetization decreased. Furthermore, the maximum values of the magnetic anisotropy were calculated as 0.3 x 10(6) erg/cc. In order to examine the difference between the in-plane magnetic anisotropy and perpendicular magnetic anisotropy, magnetic force microscopy images of the CoSiB (15-Å-thickness)/Pd (Pd thickness = 8 and 14 Å)/CoSiB (15-Å-thickness) trilayer thin films were obtained.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.