Abstract
Nanoindentation experiments are used to fabricate in a controlled manner arrays of micrometer and sub-micrometer magnetic structures at the surface of nonmagnetic, atomically ordered, intermetallic sheets with composition Fe–40 % Al (at %). The figure shows atomic (top) and magnetic (bottom) force microscopy images of these fabricated structures. The ferromagnetism arises from the deformation-induced atomic disorder in the intermetallic material.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.