Abstract

An experimental investigation was conducted to study the performance of fly ash based geopolymer mortar specimens in Magnesium Sulphate solution. Specimens were manufactured from low calcium fly ash by activation with a mixture of Sodium Hydroxide and Sodium Silicate solution and cured thermally. 10% by weight Magnesium Sulphate solution was used to soak the specimen up to 24 weeks. Performance of the specimens was evaluated in terms of visual appearance, variation of pH of solution, change in weight, and change in compressive strength over the exposure period. White deposits occurred on the surface of specimen which was initially soft but later converted to hard crystals. pH of solution increased noticeably during the initial weeks which indicate migration of alkalis from mortar specimens. At the end of 24 weeks samples experienced very little weight gain and recorded a loss of compressive strength by up to 56%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.