In Indonesia, the use of construction waste is usually not utilized properly most are simply dumped in open fields, and some are used as backfill material. The availability of such materials is vast. The purpose of this research is to determine the compressive strength value of paving blocks that utilize concrete waste with variations in the use of concrete waste, namely: 0%, 10%, 20, 30%, and the value of water absorption in paving blocks that utilize concrete waste with variations in the use of concrete waste, namely: 0%, 10%, 20, 30%. The test results showed that at 28 days of soaking, the compressive strength of normal paving blocks was 16.15 MPa, at 10% substitution of concrete waste for stone ash was 29.17 MPa, at 20% substitution of concrete waste to stone ash amounted to 39.32 MPa, and at 30% substitution of concrete waste to stone ash amounted to 22.66 MPa. From the results of the absorption test, it was found that the absorption value of normal paving blocks was 3.88%, at 10% substitution of concrete waste was 2.30%, at 20% substitution of concrete waste for stone ash was 1.89%, and at 30% substitution of concrete waste for stone ash was 2.80%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.