Background: Blood and saliva are the media for bacteria to accumulate, and it can stick to the surface of a alginate's impression during the molding process. Immersion with glutaraldehyde is one of the impression material desinfectant method since glutaraldehyde is spatially as bacterisid and fungisid. Something that must be considered when performing disinfection is the disinfection technique, as it would affect the dimension stability of impression materials. The aim of this research was to know the influence of immersion time in solution 2% glutaraldehyde disinfectant againts dimension stability. Method: The type of this research was quasi experimental using 30 samples, which were divided into five groups each containing 6 samples. The samples of alginate's impression were immersed in disinfectant solution of glutaraldehyde 2% respectively for 5, 10, 15, 20 minutes and also without immersion as the control group, then conducted a horizontal dimension stability measurement is the diameter of the die by using a digital caliper. Data were analyzed by one-way Anova test. Result: The result of this research were obtained a significance (p<0,05) between horizontal dimension stability of alginate's impression without immersed and horizontal dimension stability of alginate's impression after immersed for 5, 10, 15 and 20 minutes. Conclusion: Conclusion of this research was there was an influence of immersion time alginate's impression in disinfectant solution glutaraldehyde 2 % againts dimension stability.

Highlights

  • Blood and saliva are the media for bacteria to accumulate

  • it can stick to the surface of a alginate's impression

  • 7KH VDPSOHV of alginate's impression were immersed in disinfectant solution of glutaraldehyde 2%

Read more

Summary

Introduction

Blood and saliva are the media for bacteria to accumulate, and it can stick to the surface of a alginate’s impression during the molding process. Saat melakukan desinfeksi faktor penting yang harus diperhatikan adalah pengaruh teknik desinfeksi terhadap stabilitas dimensi bahan cetak[6], karena ketepatan hasil cetakan merupakan faktor yang sangat penting10 3HUHQGDPDQ FHWDNDQ alginat dalam larutan desinfektan iodine 1% dan isophrophyl alcohol terjadi perubahan dimensi hasil cetakan terbesar pada lama perendaman 20 menit[10]. Terdapat 1 kelompok kontrol GDQ NHORPSRN SHUODNXDQ 3RSXODVL dalam penelitian ini adalah model/die dari dental stone yang merupakan koleksi lab ).* 8QLVVXOD /DPD SHUHQGDPDQ \DQJ digunakan untuk merendam cetakan alginat di dalam larutan disinfektan glutaraldehid 2% adalah 5, 10, 15 dan 20 menit.

Results
Conclusion
Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.