Abstract

The PbSe nanocrystals were synthesized without impurity from lead oleate and Se(TOP) by heating in phenyl ether. The particle size increases the synthesis temperature. The PbSe QD / PPA nanocomposite was made with the synthesized PbSe nanocrystals and the amine-containing PPA polymer by using the ligand exchange method. The PbSe nanocrystals were well dispersed in the PbSe QD / PPA nanocomposite. The PbSe QD / PPA nanocomposite film has the broad PL peak around 1300 nm with FWHM of ~ 170 nm. The time constant in the PbSe QD / PPA nanocomposite film is as slow as ~ 150 ns. We investigated the structures of the developed PbSe QD / PPA nanocomposite film as well as their optical properties, and then suggested their photonic applications.