In order to establish the formation patterns of the Co–Mg oxide system, samples with different Co:Mg ratios and heat treatment temperatures were synthesized and studied. A study of the samples confirmed the phase transition of MgxCo2–xO4 spinels into the corresponding solid solutions at 800–900 °C. The similarity of the formation patterns for different compositions is shown. The rocksalt oxide in low-temperature samples is an anion-modified paracrystalline phase that forms a “true” solid solution only upon spinel decomposition. The TPR profiles of the decomposed Co3O4 spinel show surface Co3O4 peaks and a wide peak corresponding to the well-crystallized CoO, while partial Co3O4 TPR up to 380 °C results in dispersed and amorphous CoO. The high-temperature non-stoichiometric samples are poorly reduced, indicating their low oxygen reactivity. Spinel reoxidation after heat treatment to 1100 °C by calcination at 750 °C showed complete regeneration for MgCo2O4–Co3O4 samples and its absence in case of an excess of MgO relative to stoichiometry.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.