Abstract
The anodic behaviour and SCC susceptibility of pure copper and four α-brasses of different zinc alloy concentration in a 1 M NaNO 3 solution was studied by means of potentiodynamic polarisation curves and constant potential slow strain rate experiments. SCC was exclusively observed when the potential was equal to or higher than a certain critical value ( E c) at which pitting initiated under slow dynamic straining. It is concluded that the same SCC mechanism should be operating during SCC of copper and α-brasses in sodium nitrate, sodium nitrite and copper (II) nitrate solutions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.