AbstractPartial stabilization of Fe(II) in chemically reduced smectite, which normally readily undergoes reoxidation in air, was achieved. The purpose of this study was to determine if Fe(II) can be stabilized in reduced smectites by Li fixation upon heating. More than 80% of total Fe in ferruginous smectite SWa-1 was reduced to Fe(II) using the citrate-bicarbonate-dithionite (CBD) method while purging the clay dispersion with N2. The reduced smectite was Li-saturated, washed free of excess ions, freeze-dried, and heated in N2 atmosphere at 260°C for 24 h to produce Li-fixation. This treatment caused partial stabilization of Fe(II) in the clay structure. Chemical analysis, Mössbauer spectroscopy, and Fourier transform infrared (FTIR) spectroscopy proved that <20% of total Fe was Fe(II) after reoxidation with oxygen in a water dispersion, a treatment which causes complete reoxidation of Fe(II) in reduced Na-smectites. Decomposition of the OH-stretching band evident in the IR spectra indicated migration of Li into the vacant octahedra. Some of the OH groups in the reoxidized smectite were found in local trioctahedral configurations, associated with the AlFe(II)Li or Fe(III)Fe(II)Li groupings of central atoms in the octahedral sheet.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.