Abstract

ABSTRACTAromatic polyimide films are partially carbonized between 700°C and 1000°C. Electrical conductivity and Hall coeficient have been measured. Electrical conductivity is higher at higher measuring temperatures. The electrical conductivity σ can be expressed as σ= σ0exp (–E /kT), where k is the Boltzman constant. T is the absolute temperature. E depends upon the carborized temperature. The experimental data show the Hall coefficient RH is negative, and this implies the carriers are negatively charged, i.e. electrons. The specimens are n-type semiconductors. The carrier density η can be expressed by η= A1 exp (–E1/κT) and carrier mobility μ can be expressed by μ = A1exp ( E2/κT). E, E1andE2 depend upon the carbonized temperature

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.