Abstract
The present work is focused on finding (i) the tearing energy at rupture and (ii) the redistribution of incorporated paraffin oil on the ruptured surfaces as functions of (a) the initial oil concentration and (b) the speed of deformation to the total rupture in a uniaxially induced deformation to rupture on an initially homogeneously oil incorporated styrene butadiene rubber (SBR) matrix. The aim is to understand the deforming speed of the rupture by calculating the concentration of the redistributed oil after rupture using infrared (IR) spectroscopy in an advanced continuation of a previously published work. The redistribution of the oil after tensile rupture for samples that have three different initial oil concentrations with a control sample that has no initial oil has been studied at three defined deformation speeds of rupture along with a cryo-ruptured sample. Single-edge notched tensile (SENT) specimens were used in the study. Parametric fittings of data at different deformation speeds were used to relate the concentration of the initial oil against the concentration of the redistributed oil. The novelty of this work is in the use of a simple IR spectroscopic method to reconstruct a fractographic process to rupture in relation to the speed of the deformation to rupture.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.