Abstract

In this study the kinetic curves of cavitation wear of cast steels 20 GL and 30 L used for production of critical elements of hydraulic machines were obtained. The typical predominance of growth rate of cavitation mark diameter over its depth was found on the surfaces of the investigated cast steels. The revealed phenomenon made it possible to offer a formula for estimating the volume removal of the examined cast steels in order to expand the scope of the method according to ASTM G134-17. This method uses profilometry and microscopy and allows to determine cavitation resistance both for homogeneous and heterogeneous materials, including materials after modification of their surface (with different types of coatings and hardenings).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.