Abstract

A L27 Taguchi experiment was done to investigate the effect of laser power, welding time, laser mode (CW and two pulsed modes), focus position, and their possible interactions on the weld-bead aspect ratio of laser-welded NiTi wires by using a 100W fibre laser. The optimized parameter setting to produce the full penetrated weldment with minimum welding defects is successfully determined in the Taguchi experiment. The laser mode is found to be the most important parameter that directly controls the weld-bead aspect ratio. The focus position is the secondly important parameter for the laser welding of NiTi wires. Strong interaction between the power and focus position is found in the Taguchi experiment. The optimized weldment produced by the Taguchi experiment is mainly of columnar dendritic structure in the weld zone (WZ) with the size of 1-3µm, while the HAZ exhibits equiaxed grain structure with the size of 5-10µm. The Vickers micro-hardness test indicted that the WZ and HAZ in the weldment are softened to certain extends after fibre laser welding.A L27 Taguchi experiment was done to investigate the effect of laser power, welding time, laser mode (CW and two pulsed modes), focus position, and their possible interactions on the weld-bead aspect ratio of laser-welded NiTi wires by using a 100W fibre laser. The optimized parameter setting to produce the full penetrated weldment with minimum welding defects is successfully determined in the Taguchi experiment. The laser mode is found to be the most important parameter that directly controls the weld-bead aspect ratio. The focus position is the secondly important parameter for the laser welding of NiTi wires. Strong interaction between the power and focus position is found in the Taguchi experiment. The optimized weldment produced by the Taguchi experiment is mainly of columnar dendritic structure in the weld zone (WZ) with the size of 1-3µm, while the HAZ exhibits equiaxed grain structure with the size of 5-10µm. The Vickers micro-hardness test indicted that the WZ and HAZ in the weldment are softened ...

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.