AbstractThe authors determined conditions for manufacturing PAN precursor fibers containing a system of two nanoadditives, montmorillonite (MMT), and hydroxyapatite (HAp) in their structure. The PAN precursor fibers thus obtained are characterized by a tenacity of more than 30 cN/tex and a total volume of pores at the level of 0.29 cm3/g. Furthermore, it was found that the use of nanoadditives entails the remodeling of the paracrystalline structure of PAN fibers into a strictly crystalline one. This is accompanied by a decrease in spacing between MMT layers combined with their partial exfoliation. The fibers thus obtained, after being carbonized, will be used for medical applications. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.