Abstract

AbstractSpherical zinc gallate phosphors were prepared by using aerosol pyrolysis method. The synthetic parameters such as post heat‐treatment temperature, activator concentration, and degree of reduction were optimized for the maximum CL intensity. For enhancing the CL luminous efficiency of phosphors, adjustments of lattice structure were also considered. It was sensitive to the crystal structure in host lattice, which would be engineered by Al‐concentration in ZnGa‐Al‐O system. Zinc alumino gallates particles with spherical shape showed the brightness of 550cd/m2 with color coordinate of x=0.1665 and y=0.6655 under an excitation of 400V, 50μ/cm2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.