A supramolecular conjugate of myoglobin (Mb) and water-soluble poly(acrylate), (PA5k and PA25k , where 5k and 25k represent the molecular weight of the polymers, respectively), is constructed on the basis of a noncovalent heme-heme pocket interaction. The modified heme with an amino group linked to the terminus of one of the heme-propionates is coupled to the side-chain carboxyl groups of poly(acrylate) activated by N-hydroxysuccinimide. The ratios of the heme-modified monomer unit and the unmodified monomer unit (m:n) in the polymer chains of Heme-PA5k and Heme-PA25k were determined to be 4.5:95.5 and 3.1:96.9, respectively. Subsequent addition of apoMb to the conjugated polymers provides Mb-connected fibrous nanostructures confirmed by atomic force microscopy. A mixture of the heme-modified polymer and dimeric apomyoglobin as a cross-linker forms a microgel in which the reconstituted myoglobin retains its native exogenous ligand binding activity.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.