Abstract
This study examines the oxygen adsorption and desorption characteristics of La0.5Sr0.5Co0.8Fe0.2O3−δ (LSCF5582) membranes prepared at sintering temperatures of 1200–1300°C, with the aim of gaining an insight into their performance in the surface reaction limited regime for oxygen separation applications. The findings of this work are then compared with our experimental data on Ba0.5Sr0.5Co0.8Fe0.2O3−δ (BSCF5582) membranes. It is demonstrated that the adsorption rate constants of both membranes are two orders of magnitude greater than their respective oxygen desorption rate constants as the oxygen adsorption occurs in less than 24s whilst the oxygen desorption takes approximately one hour to reach equilibrium. The activation energy for oxygen adsorption of LSCF5582 reduced to a quarter of its value with increasing the sintering temperature from 1200°C to 1300°C. This is attributed to the oxygen exchange occurring more rapidly along the grain boundaries resulting in a lower activation energy. The LSCF5582 grain sintered at 1200°C is the optimum selection for oxygen separation applications at an operating temperature of 850°C and oxygen partial pressure of 0.21bar.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.