Abstract

In order to enhance catalytic performance for acetone, Co-based catalysts prepared under different Co/Al molar ratios and calcination temperatures have been studied in this work. The results indicated that the catalytic activities of the catalysts firstly increased and then decreased with the increase of the Co/Al molar ratio and decreased with the increase of the calcination temperature. Based on the catalytic activities, TG/DTA, XRD, TPR and XPS characterization results, it can be found that catalytic activities of the catalysts with various Co/Al molar ratios were effected by the good crystallization structure of catalyst precursor, surface Co3+/Co2+ molar ratio, low temperature reducibility, and Oads/Olatt molar ratio of the catalysts. Meanwhile, the catalytic activities of the catalysts with different calcination temperatures depended on the low temperature reducibility, surface Co3+/Co2+ molar ratio, porous structure and crystallization structure of the catalyst. Among different synthetic composition, 5:1 CoAlO-300 catalyst (T90% = 225 °C) and 5:1 CoAlO-200 catalyst (T90% = 222 °C) exhibited the efficient acetone oxidation.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call