Abstract
The oxidation behaviour of a commercial low carbon, low silicon steel in flowing air at 600-920°C was investigated. Parabolic oxidation kinetics was observed at all temperatures. Three oxidation kinetics zones with different oxidation activation energies were identified. The mechanisms responsible for the different oxidation kinetics are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.