Abstract

We investigated the oxidation behavior and the effect of the amount of SiC added on oxidation resistance in both hot-pressed ZrB 2–MoSi 2–SiC composites, 55ZrB 2–40MoSi 2–5SiC and 40ZrB 2–40MoSi 2–20SiC (vol.%), exposed to dry air at 1500 °C for up to 10 h. Quantitative electron microprobe analysis characterizations of the chemical compounds of post-oxidized composites were carried out. Parabolic oxidation behavior was observed for both composites. The addition of SiC improved the oxidation resistance of ZrB 2–MoSi 2–SiC composites, and the improvement enhanced with amount of SiC added. The microstructure of the post-oxidized composites consisted of two characteristic regions: oxidized reactive region and unreactive bulk material region. The oxidized reactive region divided into an outermost dense silica-rich scale layer and oxidized reactive mixture layer. The improvement of oxidation resistance with SiC addition is associated with the presence of a thicker dense outermost scale layer which inhibited inward diffusion of oxygen through it.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.