Abstract
The NiCrAlYSi coatings with or without Re-based diffusion barriers (DB) were prepared on K438 and K465 superalloys by electroplating Re-Ni layer, arc ion plating (AIP) NiCrAlYSi coating and following vacuum annealing. Isothermal oxidation behaviors of all coatings were investigated at 1100 ℃ in static air. The results showed that better oxidation resistance was achieved for NiCrAlYSi coatings with Re-based DB and for NiCrAlYSi coatings on K438 than that on K465. Re diffused into NiCrAlYSi coatings during isothermal oxidation and increased spallation resistance of oxide scale. The role of Re-based DB and the effects of substrate compositions were discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.