Abstract

The oxidation of an Fe-38Ni-13Co-4.7Nb-1.5Ti-0.4Si superalloy (Incoloy 909 type alloy), was investigated at temperatures between 1000 K and 1400 K in Ar-(1, 10%)H20 atmosphere using metallographic, electron probe microanalysis, and X-ray diffraction techniques. The oxide scales consist of an external scale and an internal scale which has an intergranular scale (above 1200 K) and an intergranular scale. The oxide phases in each scale are identified asα-Fe2,O3 (below 1200 K) or FeO (above 1300 K) and CoO · Fe2O3 and FeO · Nb2O5, respectively. The morphologies, the oxide phases and the oxidation rates do not depend on the partial pressure of H2O in the range between one and ten percent in Ar gas. The rate constants for the intergranular-scale formation in this alloy are about one-tenth as large as those in Fe-36%Ni alloy reported previously. At all the temperatures the scales grow according to a parabolic rate law and the apparent activation energies for the processes are estimated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.