Abstract

The feature, structure and composition of oxide films of a TP304H steel oxidized under 650°C and 25MPa water vapor for 1~50h were analyzed by SEM, EDS and XRD. The oxidizing dynamic curves were measured by discontinuous weighing method. The results indicated that the oxidation kinetics was agreement with the parabolic law. At the beginning of the oxidation, the formation of oxide was Fe2O3, while Fe3O4 and FeCr2O4 were formed with the increasing of oxidation time, without independent Cr2O3.