Abstract

The gelation behavior of Nafion dispersions was investigated using small-angle neutron scattering to better understand the mechanical toughness of dispersion-cast Nafion membranes. Three types of gelation were observed, depending on dispersing fluids: (i) homogeneous, thermally reversible gelation that was present in most aprotic polar dispersing fluids; (ii) inhomogeneous, thermally irreversible gelation as films, found in alcohols; and (iii) inhomogeneous, thermally irreversible gelation which precipitates in water/monohydric alcohol mixtures. The mechanical toughness of dispersion-cast Nafion membranes depends on the dispersing fluid, varying by more than 4 orders of magnitude. Excellent correlation between the critical gelation concentration and mechanical toughness was demonstrated with the Nafion membranes cast at 140 °C. Additional thermal effects among Nafion membranes cast at 190 °C were qualitatively related to the boiling point of dispersing fluids. Little correlation between mechanical toughne...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call