Abstract
The comparison of the low wavenumber of polarized Raman spectra (50–300 cm–1) from Bombyx mori (fresh cocoons fibres, hand‐stretched ‘Crins de Florence’ strings from the gland content, dried gland, regenerated silk films) and Nephila madagascarensis silks reveals the high polarisation of fibre modes and the absence of polarisation for dried gland and regenerated silk films. This is consistent with X‐ray diffraction measurements. The orientation of the fibroin/spidroin chains is due to the stretching during production, as for advanced synthetic fibres. The bandwidth of the ‘ordered chains’ signature is almost the same for the different fibres. However, the degree of polarisation seems to be higher in the case of spider fibre. The huge bandwidth of low wavenumber components of regenerated films indicates high disorder. Measurements along the fibre point out conformation changes with a periodicity (~20 mm) related to the silkworm head motion during the fabrication of the cocoon. Copyright © 2012 John Wiley & Sons, Ltd.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.