Abstract
The single-crystal superalloys with different deviation angle are prepared by using the liquid metal cooling high-temperature gradient directional solidification furnace, and the orientation evolution of single-crystal superalloys under different solidification interface is studied. The results indicate that the increase of the deviation angle will make the planar interface unstable. With the increase of the solidification rate, the growth direction of the crystal will deviate from the direction of heat flow to the preferred orientation direction. Under the developed dendrite crystal growth, the branches of the dendrite will follow the preferred orientation, nearly free from the effect of the heat flow.