Abstract

Recent independent experiments demonstrated that the lithiation-induced volume expansion in silicon nanowires, nanopillars, and microslabs is highly anisotropic, with predominant expansion along the <110> direction but negligibly small expansion along the <111> direction. The origin of such anisotropic behavior remains elusive. Here, we develop a chemomechanical model to study the phase evolution and morphological changes in lithiated silicon nanowires. The model couples the diffusive reaction of lithium with the lithiation-induced elasto-plastic deformation. We show that the apparent anisotropic swelling is critically controlled by the orientation-dependent mobility of the core-shell interface, i.e., the lithiation reaction rate at the atomically sharp phase boundary between the crystalline core and the amorphous shell. Our results also underscore the importance of structural relaxation by plastic flow behind the moving phase boundary, which is essential to quantitative prediction of the experimentally observed morphologies of lithiated silicon nanowires. The study sheds light on the lithiation-mediated failure in nanowire-based electrodes, and the modeling framework provides a basis for simulating the morphological evolution, stress generation, and fracture in high-capacity electrodes for the next-generation lithium-ion batteries.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.