Abstract
Polarization modulation infrared linear dichroism has been used to study the molecular orientation and relaxation of polystyrene/poly(2,6-dimethyl 1,4-phenylene oxide) (PS/PPO) miscible blends, containing up to 20% PPO, during and after a rapid uniaxial deformation above Tg. In general, it is found that both the PS and PPO chain orientation functions increase with stretching rate and PPO content, and decrease with temperature. For all blends investigated, between Tg + 5 and Tg + 13 °C, the relaxation occurs at the same rate for PS and PPO and, therefore, the relaxation times calculated are similar indicating, under those conditions, a strong relaxation coupling between the two polymers at both short and long times. © 2000 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 38: 1405–1415, 2000
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science Part B: Polymer Physics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.