This paper introduces a new and effective method for preparation of PACl-electrolysis process. A series of PACl with high content of Al 13 polymer was successfully prepared by electrolysis process. The amount of Al 13 polymer formed in electrolysis process was found to be highly influenced by current density ( d i ), the distance between the electrodes, electrolysis time and the stirring rate of the electrolyte. For the Al T (total aluminum concentration) of 2.0 M PACl obtained by electrolysis process, the optimal d i and distance between the electrodes were 1.1 A dm −2 and 10 mm respectively. The optimum circulating rate was 5.5 l h −1. Because of the inhomogeneous pH between the surface of cathode and the bulk solution, the electrolysis process has the advantage to form more Al(OH) 4 − as precursor of Al 13 polymer. At the optimum condition, Al 13 polymer accounted for above 70% of Al T (PACl of Al T=2.0 M and B=2.0), which was much higher than that of PACl prepared by other method.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.