Abstract

Psidium guajava leaves are rich in health-promoting flavonoids compounds. For better utilization of the resource, the ultrasound-assisted aqueous extraction was investigated using Box-Behnken design under response surface methodology. A high coefficient of determination (R2 = 97.8%) indicated good agreement between the experimental and predicted values of flavonoids yield. The optimal extraction parameters to obtain the highest total flavonoids yield were ultrasonic power of 407.41 W, extraction time of 35.15 min, and extraction temperature of 72.69 °C. The average extraction rate of flavonoids could reach 5.12% under the optimum conditions. Besides, HPLC analysis and field emission scanning electron microscopy indicated that the ultrasonic treatment did not change the main component of flavonoids during extraction process and the higher flavonoids content was attributed by the disruption of the cell walls of guava particles. Thus, the extraction method could be applied successfully for large-scale extraction of total flavonoids from guava leaves.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.