Abstract

A central composite design (CCD) combined with response surface methodology (RSM) was employed for maximizing bioleaching yields of metals (Al, Mo, Ni, and V) from as-received spent refinery catalyst using Acidithiobacillus thiooxidans. Three independent variables, namely initial pH, sulfur concentration, and pulp density were investigated. The pH was found to be the most influential parameter with leaching yields of metals varying inversely with pH. Analysis of variance (ANOVA) of the quadratic model indicated that the predicted values were in good agreement with experimental data. Under optimized conditions of 1.0% pulp density, 1.5% sulfur and pH 1.5, about 93% Ni, 44% Al, 34% Mo, and 94% V was leached from the spent refinery catalyst. Among all the metals, V had the highest maximum rate of leaching (Vmax) according to the Michaelis–Menten equation. The results of the study suggested that two-step bioleaching is efficient in leaching of metals from spent refinery catalyst. Moreover, the process can be conducted with as received spent refinery catalyst, thus making the process cost effective for large-scale applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.