Abstract
A method for predicting the fastest possible homogenization treatment of the as-cast microstructure of nickel-based superalloys is presented and compared with experimental results for the single-crystal superalloy ERBO/1. The computational prediction method is based on phase-field simulations. Experimentally determined compositional fields of the as-cast microstructure from microprobe measurements are being used as input data. The software program MICRESS is employed to account for multicomponent diffusion, dissolution of the eutectic phases, nucleation, and growth of liquid phase (incipient melting). The optimization itself is performed using an iterative algorithm that increases the temperature in such a way that the microstructural state is always very close to the incipient melting limit. Maps are derived allowing describing the dissolution of primary γ/γ′-islands and the elimination of residual segregation with respect to temperature and time.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.