Abstract

The Si3N4-SiC micro-nano composites were fabricated via the spark plasma sintering method using MgSiN2 as an additive. Response surface methodology and central composite design were applied to optimize the spark plasma sintering process for the fabrication of Si3N4-SiC/MgSiN2 with improved density. The relation between the three parameters of sintering including temperature, pressure, and holding time was modeled and the optimized parameters were obtained. The best sintering results obtained for the sintering temperature, holding time, and pressure are 1700°C, 487s, and 49MPa, respectively. The addition of MgSiN2 as an additive and SiC as a secondary phase were also investigated in the present work. The Si3N4−5vol% SiC composite exhibited high hardness (19GPa) and fracture toughness values (6.5MPam1/2) at room temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.