In the present study, a unique method is adopted to achieve higher reducibility of titaniferous magnetite lump ore (TMO). In this method, TMO is initially heated followed by water quenching. The quenching process generates cracks due to thermal shock in the dense TMO lumps, which, in turn, increases the extent of reduction (EOR) using the lean grade coal as a reductant. The optimum combination of parameters found by using Taguchi’s L27 orthogonal array (OA) (five factors, three levels) is − 8 + 4 mm of particle size (PS1), 1423 K of quenching temperature (Qtemp2), 15 minutes of quenching time (Qtime3), 3 times the number of quenching {(No. of Q)3}, and 120 minutes of reduction time (Rtime3) at fixed reduction temperature of 1473 K. At optimized levels of the parameters, 92.39 pct reduction is achieved. Isothermal reduction kinetics of the quenched TMO lumps at the optimized condition reveals mixed controlled mechanisms [initially contracting geometry (CG3) followed by diffusion (D3)]. Activation energies calculated are 69.895 KJ/mole for CG3 and 39.084 KJ/mole for D3.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.