Abstract

Nine types of trace nano-CeO2-doped WC-11Co cemented carbides designed by orthogonal method were prepared. The variance analysis results show that the relative density increases with increasing sintering temperature in the range of 1400-1450 °C; the hardness is highly dependent on grain size of WC which is closely related to the particle size of the initial WC powder and grain refinement produced by nano-CeO2; the bending strength of WC-11Co cemented carbide with less than 0.15 wt.% of nano-CeO2 is effectively improved because of its effect on the decreasing of porosity and inhibiting the grain growth of WC and martensitic phase transformation of Co; the fracture toughness rises at the beginning then drops later if the particle size of initial WC powder is in the range of 3-11 μm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.