Abstract
Hydroxyapatite (HA) powder was prepared by a sol–gel method using Ca(NO3)2·4H2O and (NH4)2HPO4 as raw materials. The usage of preset parameters just mixing the two raw materials only produced Ca2P2O7 and β-Ca3(PO4)2, without any evidence of HA. Then, effects of the reactant concentration, dropping speed, pH value, and mechanical stirring time on the reaction products were studied, and the process parameters were optimized. Results show that the optimum condition for the preparation of HA powder could be obtained by adding Ca(NO3)2·4H2O, (NH4)2HPO4, and citric acid to the reaction base solution, in turn, adjusting the pH value of the reaction solution with concentrated nitric acid to 2.5 and stirring the reaction solution manually. The parameters of calcination process were optimized by DSC analysis, and the HA powder with good crystallinity was successfully prepared.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.