Abstract

ABSTRACT Studies were carried out for selective leaching of Cu with simultaneous avoidance of iron dissolution during leaching of oxidized copper ore in an aqueous NH3-(NH4)2SO4 system. The effects of leaching parameters, such as ammonia concentration, ammonium sulphate concentration, leaching time, and solid-to-liquid ratio, were investigated on leaching of copper. A 2n factorial experimental design method in the dissolution experiments was used. In addition, the “Steepest Ascent” method was also applied to determine the optimum leaching conditions. It was observed that the most effective parameters on the leaching of copper were ammonia concentration and leaching time. Only 0.17% of iron in ore was dissolved in ammonia and ammonium sulphate medium. The optimum conditions established for maximum copper recovery were: ammonia concentration 2.824 mol L−1, ammonium sulphate concentration 0.236 mol L−1, solid-to-liquid ratio 0.167 g mL−1, leaching time 2 h. Fixed parameters chosen in the experiments were: room temperature, average particle size 2.8 mm, stirring speed 500 rpm. Under the optimum conditions established for maximum copper recovery, the percentage of leached copper was 98.87.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.