Abstract
Heterojunction silicon wafer solar cells, using a microcrystalline silicon (μc-Si:H) thin-film emitter and a very thin intrinsic amorphous silicon (a-Si:H) passivation layer between the crystalline silicon wafer and the emitter layer, have been reported to exhibit stable performance and high efficiency. Desired properties for the emitter layer include wide bandgap, low surface and interface recombination, and good doping efficiency. In this study, we report on the thin-film properties of p-doped μc-Si:H emitter layers deposited using RF (13.56MHz) PECVD, at different SiH4/H2 gas flow ratios, pressures, and temperatures at the same RF power. Trends relating deposition conditions to relevant film characteristics such as thickness, crystalline fraction and conductivity are discussed. Finally, device relevant symmetrical p+/i/c-Si/i/p+ heterojunction lifetime test structures are investigated, using the optimised parameters for p-doped μc-Si:H layers (discussed in this paper) and for intrinsic a-Si:H layers (discussed in a companion paper [1]). These exhibit promising effective lifetimes of up to 2.4ms at an injection level of 1015cm-3.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.