Anodic oxide coatings (AOC) formed at the potentials of spark breakdowns in aqueous solutions of potassium hexafluorozirconate (K2ZrF6) contain up to 36 wt.% of Zr. The modification of ZrO2 in AOC is tetragonal. The reflection coefficients of AOC have been measured in the range 430–670 nm. After UV irradiation for a few hours the reflection coefficient decreases by several percent. The treatment of AOC in a solution containing F− and [Fe(CN)]3− ions leads to a change in the aluminum and zirconium concentrations in the surface layer and to an increase of the AOC reflectivity.