Abstract

Optical properties of ion-beam sputter deposited SiO2–TiO2 composite films were examined in terms of composition dependence of the optical parameters, optical energy gap, and absorption character of these films. The complex refractive index of SiO2 film in the nondispersive region (λ > 310 nm) was 1.48–i0.0000, and for TiO2 (at λ > 525 nm) the index was 2.39–i0.0000 and the corresponding energy gaps 9.2 and 3.5 eV, respectively. Composite films of SiO2–TiO2 exhibited a continuous change in their optical properties. SiO2-like optical properties were dominant for the volume concentration of CTiO2≤0.25 and TiO2-like at higher concentrations.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.