92%Pb(Mg1/3Nb2/3)O3-8%PbTiO3 (PMNT) thin films have been prepared on Pt/Ti/SiO2/Si substrate with a LaNiO3 (LNO) buffer layer and on sapphire substrate by chemical solution deposition, respectively. X-ray diffraction analysis shows that the PMNT thin films on Pt/Ti/SiO2/Si substrate are almost pure perovskite phase with (110)-preferential orientation. The optical constants (n, k) of the PMNT thin films in the wavelength range of 2.5—12.6μm were obtained by infrared spectroscopic ellipsometry measurement. By fitting the optical transmission spectra of the PMNT thin films on sapphire substrate in the wavelength range of 200—1100nm, the optical constant (n and k) and absorption coefficient (α) were obtained. And that the bandgap energy of the PMNT thin films on sapphire substrate was found to be about 4.03eV.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.