La2CuO4 and La2 − xCaxCuO4 crystallites were prepared via a simple sol–gel process. The as-prepared La2CuO4 and La2 − xCaxCuO4 crystallites were characterized by X-ray diffraction, transmission electron microscope and UV–vis–NIR spectra. Results show that the grain size of La2CuO4 crystallites increases with the increase of heat treatment temperature from 600 °C to 800 °C. Optical properties show that La2CuO4 crystallites have broad absorption both in the UV–vis region and in the NIR region. The band gap of the as-prepared crystallites decreases from 1.367 eV to 1.284 eV with the increase of calcination temperature from 600 °C to 800 °C. In the series of La2 − xCaxCuO4 compounds (x = 0.05, 0.08, 0.10, 0.12, 0.15 and 0.20), all of the samples exhibit an orthogonal crystal structure and the solubility limit of Ca2 + in La2CuO4 is within the range of x = 0.12–0.15. In the whole UV–vis–NIR region, La2 − xCaxCuO4 crystallites exhibit a broad absorption and the corresponding band gap first increases and then decreases with increasing of Ca2 + content.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call