Abstract

Undoped and Fe-doped (Fe ions content was 0.1) TiO2 thin film prepared by Sol-gel method. X-ray diffraction (XRD) results showed that TiO2 gel annealed at 500°C was crystallized anatase phase. The contact angle for undoped and Fe-doped TiO2 thin film was 47.1° and 8.8°. The transparent spectra showed that the cutoff wavelength of was red shift. The band-gap of Fe-doped TiO2 film was 3.47 eV.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.