Abstract

ZnO + Zn2TiO4 thin films were obtained by the sol–gel method using precursor solutions with different Ti/Zn ratios in the 0.18–2.13 range. The films were deposited on glass substrates and annealed in an open atmosphere at 550 °C. The oxide was characterized by X-ray diffraction and photoacoustic (PA) spectroscopy. The films were constituted of polycrystalline ZnO for the lowest Ti/Zn ratio (0.18), polycrystalline Zn2TiO4 for the 0.70 and 1.0 ratios, and mixes of both oxides for the intermediate ratios (0.32 and 0.50). For the highest ratios studied (1.44 and 2.13), the films were amorphous. The energy band gap (Eg) values were determined from optical absorption spectra, measured by means of the PA technique spectra. Eg varied in the 3.15 eV (ZnO) to 3.70 eV (Zn2TiO4) range.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.