Thin films of InTe and InSe were obtained by the discrete evaporation of pure material from a tantalum boat in a vacuum of 4 × 10 −6 torr, onto well cleaned glass substrates. The deposition temperature was varied from 303 to 573 K. Optical absorption of the films was recorded in the range 13000 to 3000 cm −1 and the data was used to deduce optical energy gap of the films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.