Abstract

We demonstrate that titanium (IV) oxide films may be deposited on Corning glass by a simple, one-pot, low temperature (95 °C) hydrothermal growth technique and that providing the correct conditions are employed, the films produced show clear photoactivity under UV illumination as evidenced by changes in water contact angle and the progressive photo-oxidation of stearic acid. It is further demonstrated that the growth, structure and photoactivity of the films depends critically upon the H 2O concentration employed during growth. For H 2O concentrations below 0.1 M, little or no growth was observed, while above 0.3 M, precipitation or even gelation rapidly occurred. Only at H 2O concentrations of 0.1 M and 0.2 M was appreciable film growth observed, while photoactive titania was formed only via growth using a water concentration of 0.1 M, the films grown using the higher concentration of water (0.2 M) being essentially photo-inactive. The method developed is discussed in terms of the possible chemical steps involved and is proposed as a low-cost alternative to higher temperature, less environmentally friendly approaches to TiO 2 film production.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.